46 C.F.R. § 154.172
(c) If a steel grade that is not listed in Table 1 has the equivalent chemical properties, mechanical properties, and heat treatment of a steel grade that is listed, the steel grade not listed may be specially approved by the Commandant (CG-ENG), for use in the contiguous hull structure.
| Minimumtemperature | Steel thickness | Steel 1 grade |
|---|---|---|
| 0 °C (32 °F) | All | Standards of the American Bureau of Shipping published in “Rules for Building and Classing Steel Vessels”, 1981 |
| −10 °C (14 °F) | T≤112.5 mm (1⁄2 in.) | B |
| 12.5<t≤25.5 mm (1 in.) | D | |
| >25.5 mm (1 in.) | E | |
| −25 °C (−13 °F) | t≤112.5 mm (1⁄2 in.) | D |
| >12.5 mm (1⁄2 in.) | E | |
| 1 Steel grade of the American Bureau of Shipping published in “Rules for Building and Classing Steel Vessels”, 1981. |
[CGD 74-289, 44 FR 26009, May 3, 1979, as amended by CGD 82-063b, 48 FR 4782, Feb. 3, 1983; CGD 77-069, 52 FR 31630, Aug. 21, 1987]